This is because the heating time is shortened to make the width of the edge heating zone narrower to shorten the time for forming the metal oxide. The size of the opening angle is related to the stability of the burning process, which has a great influence on the welding quality.If the welding speed is decreased, not only the heating zone becomes wide but also the width of the melting zone varies with the input heat amount, burr larger.
The welding speed is also one of the main parameters of the welding process, which is related to the heating system, the deformation Auto parts plastic welding machine speed of the welding seam and the mutual crystallization speed. The actual production experience shows that the longitudinal position of the movable guide roller to adjust the size of the opening angle, usually between 2 ~ 6 ° change. In low-speed welding, the heat input less difficult to weld, if not meet the required value prone to defects. Under the other conditions, the heating temperature of the edge can be increased and the welding speed can be increased. If the opening angle is too small, the distance from the meeting point to the center line of the squeezing roller will be lengthened, resulting in the edge being not squeezed at the highest temperature, thus reducing the welding quality and increasing the power consumption.
Due to the possible tolerances of the erw tube width and thickness, as well as fluctuations in the welding temperature and welding speed, changes in the welding pressure may be involved. In the erw pipe, the welding quality increases with the welding speed.
The opening angle refers to the angle between the two edges of the tube before the squeeze roll. When the opening angle is decreased, the distance between the edges is also reduced, so that the adjacent effect is strengthened. Therefore, in the erw pipe, should be in the unit of the maximum allowable speed of mechanical equipment and welding equipment, according to different specifications of the species to choose the right welding speed. The amount of welding extrusion is generally controlled by adjusting the distance between the squeeze rollers, or it can be controlled by the difference in the circumference of the squeeze rollers before and after. In the case of the guide roller can not be adjusted vertically, you can use the thickness of the guide ring Ultrasonic Plastic Welding machine or press the closed hole to adjust the size of the opening angle
0コメント